INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Thermowell with NACE MR0103 Compliant

Thermowell with NACE MR0103 Compliant

Thermowell with NACE MR0103 Compliant

(OP)
I have manufacture an thermowell under Nace mr103 but I dont understand this standard.
The thermowell will be in AISI 316 but I don´t Know which care I have for this.
anyone AISI316 or 316L is compliant????

Thanks in advance

RE: Thermowell with NACE MR0103 Compliant

MR0103 addresses austenitic stainless steels with carbon content up to 0.1 mass%.  Therefore, both 316L and 316 are addressed under the requirements of 2.5.1

Steve Jones
Materials & Corrosion Engineer
http://www.linkedin.com/pub/8/83b/b04
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources