Does anyone know the correct AWS designation for welding the casting alloy A356? Casting specs are AMS-4218, ASTM B26, B108, AMS-A-21180?
Thanks
Thanks
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
A356 Al weld rod designation
|
RE: A356 Al weld rod designation
Use GTAW
AWS SFA 5.10
For welding actual A356 the rod would be
R-A356.0