INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Pick Up Effects on Al Extrusion

Pick Up Effects on Al Extrusion

Pick Up Effects on Al Extrusion

(OP)
Dear Expert Friends,

Some of our products, have pick up marks(defects) on them. We're observing pick-up effects during and after the extrusion process. I'm trying to solve this problem so I'm open for ideas and tips.

Thanks  

RE: Pick Up Effects on Al Extrusion

Can you provide some additional details on the exact nature of these defects?  Size, location, etc.?  Die construction, materials, heat treatment, surface treatment, etc.?  The following has some descriptions of defects:

http://faculty.kfupm.edu.sa/coe/sadiq/proceedings/SEC2002/vol5/P137.pdf


Two other recent contributions on defects in Al extrusions were authored by Alcan and the University of Queensland:

Classification of Streaking Defects on Anodized Aluminium Extrusions
http://www.scientific.net/MSF.618-619.349

Effect of primary intermetallic particles on surface microstructure and appearance of aluminium extrusions
http://www.sciencedirect.com/science?_ob=ArticleURL&_udi=B6TX4-4TCGKW6-9&_user=10&_rdoc=1&_fmt=&_orig=search&_sort=d&_docanchor=&view=c&_searchStrId=992068525&_rerunOrigin=scholar.google&_acct=C000050221&_version=1&;_urlVersion=0&_userid=10&md5=58a143d2bf29536d5d73dead3f35d917

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources