INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

welding rebar

welding rebar

welding rebar

(OP)
I have a client who operates a precast facility,he wants to get certified to weld A706 rebar ,I advised against it ,but he wants to move ahead, anyone know of a good reference.  

RE: welding rebar

I'm curious, why advise against it?  I know of precasters who weld up their own embed plates with A706 bars.  I imagine it saves the time and markup of having them fabricated elsewhere.

As for references, I'd start with AWS, AISC, PCI...

RE: welding rebar

AWS D1.4 is the welding code for reinforcing steel.   

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources