INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

316L : Impact toughness values at low temperatures
2

316L : Impact toughness values at low temperatures

316L : Impact toughness values at low temperatures

(OP)
Hi

Can anybody can show me a good link for the impact toughness values to the 316L grade at low temperatures (-20,-30,-40,.....  up to -80°C)
Thanks in advance

Stan

 

RE: 316L : Impact toughness values at low temperatures

(OP)
Great

Metenger you are a good guy !
 

RE: 316L : Impact toughness values at low temperatures

stanislasdz we regularly test at -196 Deg C and get 100K plus

RE: 316L : Impact toughness values at low temperatures

(OP)
100K ?????

sorry russ8910 i don't understand this unit ?

I expected values in joules  

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources