How to predict the ferrite content in the 9%Cr-1%Mo steel (P91) ?
How to predict the ferrite content in the 9%Cr-1%Mo steel (P91) ?
(OP)
How to predict the ferrite content in the 9%Cr-1%Mo steel (P91)
Thanks
Thanks
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
How to predict the ferrite content in the 9%Cr-1%Mo steel (P91) ?
|
RE: How to predict the ferrite content in the 9%Cr-1%Mo steel (P91) ?
You can predict ferrite content by obtaining a CCT diagram for this steel. They are available. You can also contact V&M for this information.
RE: How to predict the ferrite content in the 9%Cr-1%Mo steel (P91) ?
Have a look on page 7 on this paper
ht
can you tell me the accuray of this formula ?
RE: How to predict the ferrite content in the 9%Cr-1%Mo steel (P91) ?
Looks interesting and I will read the paper. I would still contact V&M because they have been producing Grade 91 material for years. They would be very helpful in this area.
RE: How to predict the ferrite content in the 9%Cr-1%Mo steel (P91) ?