Searching for: glulam utility pole design guide and/or tapered rectangular bending member design-cantilever. Have AITC Handbook, ANSI O5.1 and ANSI O5.2, ASCE 111 and NESC.





RE: Glulam utility pole design information
RE: Glulam utility pole design information
RE: Glulam utility pole design information
Three ASTM standards are related to wood poles and piles (primarly round). The main standard, designated D3200 ,refers to two other standards: ASTM D25, Standard Specification for Round Timber Piles and ASTM D2899, Standard Pracitice for Establishing Design Stresses for Round Timber Piles