*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Coating breakdown: DnV RP F103 vs. DnV RP B401

Coating breakdown: DnV RP F103 vs. DnV RP B401

Coating breakdown: DnV RP F103 vs. DnV RP B401

(OP)
the coating breakdown coefficients (a and b) in DnV-RP-B401 where in order of 0.1 and 0.01.
these coefficient are remained unchanged in new revision of B401.
on the other hand, the DnV-RP-F103 proposes very different coefficients, which are in order of 0.001 and 0.0001; which leads to very light anodes.
What is the problem? It doesn't seem to be correct and I smell a rat in this approach???  

RE: Coating breakdown: DnV RP F103 vs. DnV RP B401

Same answer to the same question that you also posted in the offshore structure/pipeline engineering forum!!

Steve Jones
Materials & Corrosion Engineer
http://www.linkedin.com/pub/8/83b/b04
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources