Looking for high purity OFC copper
Looking for high purity OFC copper
(OP)
Hi,
I am having difficulties locating high purity OFC copper 101. The material probably has to be custom made as the difficult requirement is for VERY LOW impurities. In rod shape of less than 2" diameter.
Any ideas?
Thanks!
I am having difficulties locating high purity OFC copper 101. The material probably has to be custom made as the difficult requirement is for VERY LOW impurities. In rod shape of less than 2" diameter.
Any ideas?
Thanks!





RE: Looking for high purity OFC copper
There are companies that specialize in small amounts of high purity metals.
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
RE: Looking for high purity OFC copper
http://ww
RE: Looking for high purity OFC copper
RE: Looking for high purity OFC copper
Ed, I need about 30 meter of one thickness and 10 meter of other thicknesses. Do you have a source? I have a list of impurities allowed. The regular OFC copper 101 does not cut it.
Luvata, I think that they could do it but they only work with very large diameters. I am looking for mostly less than 2" diameter. TVP, thanks for the tip.