INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Compressive Strength of Concrete Volumetric Base

Compressive Strength of Concrete Volumetric Base

Compressive Strength of Concrete Volumetric Base

(OP)
Dear All,

What is the maximum cylindrical compressive strength that can be achieved, basing on volumetric mix of concrete as follows.

1. 1:2:4
2. 1:1.5:3
3. 1:4:8

I would seek your expert opinion on if it is possible to achieve 3000 Psi cylinder strength using OPC and mix ratio (1:2:4) and 3750 Psi cylinder strength using OPC and mix ratio being (1:1.5:3) with out using any construction chemicals additionally.

Regards,  

Engr. Shakeel Ahsan
Director Engineering
CMEC - Pakistan

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources