ASME Section 2 Part D table 5A
ASME Section 2 Part D table 5A
(OP)
I can't find A992 Gr 50 in ASME Section 2 Part D table 5A - for I-Beams in high temperature service (750 DegF). Is it there and I am missing it? Does anyone have a different source?





RE: ASME Section 2 Part D table 5A
BTW, I am looking at ASTM A-992-04a and only see a single grade.
Regards,
Mike
RE: ASME Section 2 Part D table 5A
The table includes SA-675 of various grades and SA-36 for "shapes" but does not include A573 or A992.
Would I be remiss in using the reduction factors for 675-50 for A992?
Where might I find strength reduction factors for A992?
Where might I find Young's Modulus temperature reduction factors?
This is old, but short: http://w
RE: ASME Section 2 Part D table 5A
Here's an ASCE presentation...
http://
Or you could buy this one...
htt
RE: ASME Section 2 Part D table 5A