damage concrete steel reinforce piles & beam
damage concrete steel reinforce piles & beam
(OP)
how can i best repair these piles. the head supporting the beams are damage an showing some of the steel which are corroded and flaking concrete. this is all above the water line





RE: damage concrete steel reinforce piles & beam
Steve Jones
Materials & Corrosion Engineer
http://www.linkedin.com/pub/8/83b/b04