Fuel safe RTV or castable rubber?
Fuel safe RTV or castable rubber?
(OP)
Im trying to make a part of which common pourable RTV silicone is ideal as it needs to be cast. Only problem is it must be reasonably fuel (gasoline) resistant which all RTV's I've tried are not.
It's doesn't need to be silicone. Any rubber about 30 Shore hardness will do.
Thanks.
It's doesn't need to be silicone. Any rubber about 30 Shore hardness will do.
Thanks.





RE: Fuel safe RTV or castable rubber?
In that case can anyone tell me where to obtain sheet, or block/bar stock of fuel resistant rubbers?
Thanks.
RE: Fuel safe RTV or castable rubber?
A quick Google search yielded a site:
http://ww
Good luck!
tom