INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASTM A666 Free Bend Requirements

ASTM A666 Free Bend Requirements

ASTM A666 Free Bend Requirements

(OP)
Customer drawing calls for minimum bend radius on 304 ASTM A666 stainless steel. ASTM specifications give a Bend Factor of 1 for Thicknesss>0.050 to <= 0.1874in. for Free Bending and Bend Factor of 3 for V-Block Bending. Is air bending regarded as "Free Bending"?

 

RE: ASTM A666 Free Bend Requirements

It is usually done with guides, but it isn't like between dies.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources