INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Piezo material properties for ANSYS

Piezo material properties for ANSYS

Piezo material properties for ANSYS

(OP)
Hi,
In ANSYS you can import material properties of piezo ceramics. But where can I find the specific material properties that are required by ANSYS?

You can find all kind of piezoelectric material properties on the net, like:
http://www.efunda.com/materials/piezo/material_data/matdata_output.cfm?Material_ID=PZT-8

or

http://www.matweb.com/search/DataSheet.aspx?MatGUID=ce802bd7a06b4b2f9f539e7c2c141f75

however, those are not compatible with what ANSYS requires. Where can I find the data that ANSYS requires?

The data that ANSYS needs:
! Material properties for PZT-4
!
mp,DENS,1,7700                 ! Density, kg/m**3

tb,DPER,1                      ! Relative permittivity at constant strain
tbdata,1,729,635,729
! - Alternative input of permittivity if used with SOLID5
! mp,PERX,1,729
! mp,PERY,1,635
! mp,PERZ,1,729
!
tb,ANEL,1                      ! Anisotropic elastic stiffness, N/m^2
tbdata,1,13.9E10,7.43E10,7.78E10  ! c11,c13,c12
tbdata,7,11.5E10,7.43E10       ! c33,c13
tbdata,12,13.9E10              ! c11
tbdata,16,2.56E10              ! c44
tbdata,19,2.56E10              ! c44
tbdata,21,3.06E10              ! c66

tb,PIEZ,1                      ! Piezoelectric stress coefficients, C/m^2
tbdata,2,-5.2                  ! e31
tbdata,5,15.1                  ! e33
tbdata,8,-5.2                  ! e31
tbdata,10,12.7                 ! e15
tbdata,15,12.7                 ! e15

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources