Data sheet for FM96 Adhesive
Data sheet for FM96 Adhesive
(OP)
Howdy all,
Does anyone have a datasheet for Cytec FM96 adhesive? We have a reference in a DC10 drawing, but it looks like it is no longer used. Cytec has only one line on their website about it that indicates it's a 350° cure modified epoxy. Thanks.
-Kirby
Does anyone have a datasheet for Cytec FM96 adhesive? We have a reference in a DC10 drawing, but it looks like it is no longer used. Cytec has only one line on their website about it that indicates it's a 350° cure modified epoxy. Thanks.
-Kirby





RE: Data sheet for FM96 Adhesive
Couldnt find a data sheet, but was able to find lap shear strengths in the NASA Non-Metallics Manual.
RE: Data sheet for FM96 Adhesive
Thanks, that is exactly what I was needing. Looks like a lot of other good info in there as well. I also like that it is a NASA report. For material data I trust that.