INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Fire rating of ordinary gypsum boards
2

Fire rating of ordinary gypsum boards

Fire rating of ordinary gypsum boards

(OP)
Pals

manufacturers have tables for ratings of walls made from fire resistant gypsum boards. In US such FR gypsum boards are usually type X gypsum boards. In Europe they have a similar type.

I would like to be able to determine fire ratings of an ordinary gypsum boards

respects

IJR

RE: Fire rating of ordinary gypsum boards

Typically a 1/2-inch drywall with 3 1/2-inch stud wall will yield a 15-minute fire resistance rating, but is still dependant on installation quality.

You can also browse the UL certifications site at UL.com for differant gypsum wall types/construction types for the various fire ratings.

RE: Fire rating of ordinary gypsum boards

The thickness of the layer is important but so is its orientation and application. The requirements vary if you are designing a fire wall, fire barrier or horizontal barrier under the requirements of the 2006 IBC.

Go to the US Gpysum Association website and download GYP-600, which is the fire resistive construction directory for all things gypsum. I would send you a link but I am in the airport and my laptop battery is about to die.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources