Strength of Plug Welds
Strength of Plug Welds
(OP)
Does anyone know where to find a design guide or a procedure for determining the strengh of plug welds?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Strength of Plug Welds
tg
RE: Strength of Plug Welds
Plug welds can be treated like fillet welds. If you know the size of the weld, weld metal type you have all of the essential variables necessary to determine the allowable stress per unit length of weld under tension (based on weld metal ultimate tensile strength) and shear (50% of the ultimate tensile strength as and approximation).