SAE equivalent ASTM A 656?
SAE equivalent ASTM A 656?
(OP)
Actually I need the fatigue data for A 656, but if there is a SAE equivalent, perhaps it is in my material database.
Is there any site that just lists equivalencies?
And a broader question is if you don't have fatigue data, and you don't have an equivalent's fatigue data, what is the best way to guess fatigue properties.
Some people find fatigue data which has matching ultimate tensile strength. But my experience is that ultimate tensile strength and fatigue life don't correlate very well.
Is there any site that just lists equivalencies?
And a broader question is if you don't have fatigue data, and you don't have an equivalent's fatigue data, what is the best way to guess fatigue properties.
Some people find fatigue data which has matching ultimate tensile strength. But my experience is that ultimate tensile strength and fatigue life don't correlate very well.





RE: SAE equivalent ASTM A 656?