What the materials (ASTM or AISI) that generally use for casing head housing (refer to API 6A-75k-AA Class)?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Wellhead's Material
In general, however, 4130 is used. Slight variations may be used by specific manufacturers, but most of them are 4130.