Could someone give me examples of what pyroxylin plastic is used in? Specifically those items that would fall under NFPA 42.
Thanks for the help
Thanks for the help
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Pyroxylin plastic
Any other uses have been discontinued or most likely destroyed by fire as pyroxylin plastic is easily ignited.