INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

CWI Stamp

CWI Stamp

CWI Stamp

(OP)
Is it necessary for a WPQ Welders Cert to be stamped with a CWI stamp and is it stated anywhere.

RE: CWI Stamp

It is necessary only if required by the contract.  It is not required by AWS specifications.

RE: CWI Stamp

(OP)
Is this stated in AWS,ASME or anywhere else.

RE: CWI Stamp

NO, it is not stated.

Not stated....don't have to do it

RE: CWI Stamp

(OP)
Thanks
Then when can we use the stamp

RE: CWI Stamp

Quote:

Then when can we use the stamp

Doesn't hurt anything at all to have a CWI stamp on WPQs, WPSs, PQRs....you can stamp these documents.

 

RE: CWI Stamp

There is no requirement by AWS to ever use a stamp. Some contracts/job specs will want reports, PQR's, and WPS' to be stamped by a CWI.

RE: CWI Stamp

Makes sense to stamp the WPQ's if you need the WPQ's on future projects. Codes may change, and some clients will only approve WPQ's approved by a third party organization.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources