Hi every one,
I have to do damage modelling for a complex composite material, so just to check if it's going to work in ANSYS
I modelled a simple curved geometry of two curved materials (of similar properties or different), meshed with solid185 elements and seperated by interface elements.
But here I have problem with convergence just before reaching maximum normal stress of interface elements (INTER205). I tried with different element formulations also but still have this convergence problem. Please note that I am not looking for accuracy in this case and so the model is not meshed fine at the curves (does it affect the conrgence?).
Please help me find where I am going wrong, this is very important for my work.
I am attaching the input file for this problem for your understanding, please try this.
Thanks a lot for your inputs,
Vinston
I have to do damage modelling for a complex composite material, so just to check if it's going to work in ANSYS
I modelled a simple curved geometry of two curved materials (of similar properties or different), meshed with solid185 elements and seperated by interface elements.
But here I have problem with convergence just before reaching maximum normal stress of interface elements (INTER205). I tried with different element formulations also but still have this convergence problem. Please note that I am not looking for accuracy in this case and so the model is not meshed fine at the curves (does it affect the conrgence?).
Please help me find where I am going wrong, this is very important for my work.
I am attaching the input file for this problem for your understanding, please try this.
Thanks a lot for your inputs,
Vinston





RE: Convergence problem - help needed urgent pls
RE: Convergence problem - help needed urgent pls
Thanks for your time,
Vinston
RE: Convergence problem - help needed urgent pls