INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Braze alloy for Carpenter Custom 465 SS?

Braze alloy for Carpenter Custom 465 SS?

Braze alloy for Carpenter Custom 465 SS?

(OP)
Does anyone have any recommendations for a biocompatible brazing alloy that works well with Carpenter Custom 465 SS and 316L SS?  Thanks.

RE: Braze alloy for Carpenter Custom 465 SS?

Ask Cartech.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube

RE: Braze alloy for Carpenter Custom 465 SS?

(OP)
Hi Ed,

Thanks for the reply.  Unfortunately Cartech doesn't have a west coast office and they close at 5PM EST (2PM local).  I was hoping to find an alloy and not wait till tomorrow, esp since there's no guarantee cartech will have a suggestion.  My brazing guy is having bad luck with the BAu-4 and needs to try something else.  Any ideas?

RE: Braze alloy for Carpenter Custom 465 SS?

I would have suggested a Ni/Au alloy, looks like you are going that way.  Is the brazing guy using a reducing atmosphere?  If not, what flux is he using?

RE: Braze alloy for Carpenter Custom 465 SS?

The real trick is finding a braze alloy so that the braze temp matches the required heat treat temp.
Find the heat treat temp and then search the braze alloys.  You will sacrifice quality and strength in order to just get a joint that doesn't ruin the 465.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources