INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Chloride Attack of Concrete
2

Chloride Attack of Concrete

Chloride Attack of Concrete

(OP)
I previously worked on project were the bridge piers of a highway passing over a major dual carriageway had been attacked by chloride.  The road was subject to sub-zero conditions and a chlorine based de-icier was used to stop the road from freezing.  The sub-grade of the road was slag, a by product of burning coal in power stations with good engineering properties.  But the combination of the slag and the chloride attacked the concrete to the piers rapidly and cause the concrete to become extremely weak.  I think the process or chemical reaction is called Thauximite.  But I need conformation on this and also what was the chemical reaction between the slag, chlorine and concrete.  Thanks is advance for any suggestions.

RE: Chloride Attack of Concrete

Hello Rich,

It sounds a little like thaumasite sulfate attack.  The samples of it that I have sitting on my desk (I am a very sad person) show bands of white through the concrete and are easily damaged by fingernails.  

I have only had a brief contact with this sort of problem but WS Atkins (Britain), maintaining agents for the Highways Agency Area 2 (near Bristol) have a lot of experience regarding this subject.  There has been several conferences and and papers on this problem but I confess I can't give you any guide here.

RE: Chloride Attack of Concrete

RichinEthiopia,

You might consult

www.bre.co.uk

This is the website of the Building Research Establishment in the UK.  Follow the links to Concrete or the links to the BRE Bookshop.

Similarly

www.trl.co.uk

is the website of the UK Transport Research Laboratory from which I copied the following publication details.  You should visit the website yourself to obtain a more suitable search result.

The influence of chlorides on the alkalinity of concrete
Report No. LR 915
Author(s): P R Vassie. 1979
Price: £20.00

An international review of chloride ingress into structural concrete. 1997
Report No. CR359/BR
Author(s): P B Bamforth, W F Price, M Emerson
Price: £30.00

Methods to determine chloride concentrations in in-situ concrete. 1986
Report No. CR32
Author(s): J W Figg
Price: £20.00



Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources