INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

13% Chrome vs. Super 13% Cr

13% Chrome vs. Super 13% Cr

13% Chrome vs. Super 13% Cr

(OP)
I beleive the 13 Cr is the same as Grade 420 modified, but what about Super 13 Cr? Does it have the same chemical composition as 13 Cr? What is the values for yield, tensile on this material?

Regards

Tommy

RE: 13% Chrome vs. Super 13% Cr

(OP)
I beleive the SM13CRS grade has 95 ksi yield?! Are you sure this is the Super 13 Cr? The 420 modified (13 Cr) has a yield stress of 110 ksi (NACE approved).

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources