catalytic reformer unit
catalytic reformer unit
(OP)
BPP means barrel of feed per pound of catalyst.Sometimes this is given as m3/kg in metric unit. Can anybody show me how the catalyst life is calulated in these units or any of them?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: catalytic reformer unit
1) The total amount of catalyst loaded in Kg
2) The accumulated feed to the plant. for example, if you have been treating 60 m3/h of heavy nafphta for one day, the accumulated feed would be 60m3/h x 24 h= 1440 m3
Then, the "life" of the catalyst is 1440 m3/Amount of cat.
Hope this is clear enough
RE: catalytic reformer unit
Also that will mean the catlayst life is constant.
I will appreciate further elucidation.