INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

PPlication of Aluminum Brass B148-955 in sour water service

PPlication of Aluminum Brass B148-955 in sour water service

PPlication of Aluminum Brass B148-955 in sour water service

(OP)
Does anyone have experience in the application of Aluminum Brass alloy B148-955 in centrifugal pumps for refinery sour water service. Severe housing and impeller   corrosion has been experienced. Would like to know what material will be best for this service.
Thanks
 

RE: PPlication of Aluminum Brass B148-955 in sour water service

316/316L will be a starting option in alkaline sour water.  If the water is acidic with chlorides (probably not otherwise you would not have lost the  nickel aluminium BRONZE), ISO 13709, Material Class D-1, duplex stainless steel should do.

Steve Jones
Materials & Corrosion Engineer
http://www.linkedin.com/pub/8/83b/b04
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources