INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Extrusion Alloy 7129 Mechanical Props requested

Extrusion Alloy 7129 Mechanical Props requested

Extrusion Alloy 7129 Mechanical Props requested

(OP)
Hi Everyone,  Does anyone have any mechanical properties (UTS, yield,elongation) for 7129 aluminum alloy as it applies to extrusions?  The higher T tempers are what I would be interested in.  My references are not new enough to have it, and I'm not having a lot of luck finding it on the internet.  Thanks.

RE: Extrusion Alloy 7129 Mechanical Props requested

T5,T6 typical:
430 MPa UTS
380 MPa YS
15% El
270 MPa Shearing Strength
-Alcoa 1987
 

RE: Extrusion Alloy 7129 Mechanical Props requested

(OP)
Thanks Flesh.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources