Wide flange W12X10x58 properties
Wide flange W12X10x58 properties
(OP)
Hello,
can anybody point me in the right direction. I am trying to find (on the internet) the properties of the above mentioned section, but have only come up with W12x4x22 as the largest section mentioned:
http://www.spemweb.info/profile.php
Just need basic values, nothing fancy.
Does anybody know a website that lists section properties including the one mentioned above?
Thanks
can anybody point me in the right direction. I am trying to find (on the internet) the properties of the above mentioned section, but have only come up with W12x4x22 as the largest section mentioned:
http://www.spemweb.info/profile.php
Just need basic values, nothing fancy.
Does anybody know a website that lists section properties including the one mentioned above?
Thanks






RE: Wide flange W12X10x58 properties
Type: W
ID = 215
Designation = W12X58
W = 58
A = 17
D = 12.2
BF = 10
TW = 0.36
TF = 0.64
T = 9.25
KDES = 1.24
KDET = 1.5
K1 = 0.9375
BF_2TF = 7.82
H_TW = 27
FY3P = 0
X1 = 3070
X2 = 1470
IX = 475
ZX = 86.4
SX = 78
RX = 5.28
IY = 107
ZY = 32.5
SY = 21.4
RY = 2.51
J = 2.1
CW = 3570
WNO = 28.9
SW = 46.3
QF = 17.8
QW = 42.4
RE: Wide flange W12X10x58 properties
http://www.slideruleera.net/miscellaneous.html
Download "Bethlehem Structural Shapes Catalog - 1948", and look on page 25.
I have several older references that list the properties of numerous steel shapes from days gone by.
www.SlideRuleEra.net![[idea] idea](https://www.tipmaster.com/images/idea.gif)
www.VacuumTubeEra.net
RE: Wide flange W12X10x58 properties
Very helpful.