Crude Oil w/ Vanadium & Sodium
Crude Oil w/ Vanadium & Sodium
(OP)
Hi,
Designing a heating unit to raise the temperature of #6 oil containing sodium & vanadium to about 265 deg F. Will carbon steel corrode under these conditions or should 304 stainless be used for the construction?
Thanks
Designing a heating unit to raise the temperature of #6 oil containing sodium & vanadium to about 265 deg F. Will carbon steel corrode under these conditions or should 304 stainless be used for the construction?
Thanks





RE: Crude Oil w/ Vanadium & Sodium
For the temperature you said carbon steel will be good enough.
luis marques
RE: Crude Oil w/ Vanadium & Sodium