INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

SA 541 help

SA 541 help

SA 541 help

(OP)
Can anybody please help me find thermal conductivity of SA 541 grade 3 (uns K12045)
Any additional info would also be greatly appreciated.
All my attempts to search online drew a blank!
thanks!

RE: SA 541 help

Table TCD of ASME Section II Part D lists nominal coefficient of thermal conductivity for various materials. SA-541 grade 3 belongs to Material Group C in that table. Values for thermal conductivity are listed as a function of temperature so it's a long list. What's the temperature?

RE: SA 541 help

(OP)
around 200-300C.

RE: SA 541 help

200 °C  -  40.1 W/m-°C
250 °C  -  39.5 W/m-°C
300 °C  -  38.7 W/m-°C

RE: SA 541 help

(OP)
Thanks!

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources