INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Full killed carbon steel and Sour...

Full killed carbon steel and Sour...

Full killed carbon steel and Sour...

(OP)
Dear sir

I'd like to your explain these item below.
1. Full killed carbon steel
2. killed cabon steel
3. sour service H2s
4. Cs+NACE MR0175

RE: Full killed carbon steel and Sour...



Killed Carbon Steel is a process of deoxidation that is performed during the steel making process. Normally, ASME B&PV Code requires steels that have 0.24% or greater carbon contents to be killed (fully de-oxidized) using either Al or Si additions, and especially those steels that fall under a forging grade.

For sour service and NACE MR0175 go to

http://www.genel-makina.com/2008/pdf/bulten1155.pdf

lm

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources