Does material JISG3131-SPHC and ASTM A36 are equivalent?
Here, equivalent is limited to mechanical properties, chemical composition and others testing requirements not for Code or Standard judgment
Here, equivalent is limited to mechanical properties, chemical composition and others testing requirements not for Code or Standard judgment





RE: JISG3131 SPHC VS ASTM A36
RE: JISG3131 SPHC VS ASTM A36
I have tried to compare both of them, but I can't find both are "typical" material based on chem analysis & mech properties. There some properties different to much.
Can you help me to determined both are "equivalent"
RE: JISG3131 SPHC VS ASTM A36
What is the application where you want to substitute the A36 for G3131? The attachment you provided is not complete with the necessary information.