For SAW, can flux used for PWHT be used for non-PWHT welding? For example, can F7P2 designation be used for Non-PWHT welding?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: SAW welding flux
Lincoln certifies certain wire flux combinations with and without PWHT. eg. LA-71 /880M ( P6 A6 )