316 L
316 L
(OP)
Hi All
Does anyone tell me what kind of 316 L tubes weld inspection according to ASME? I was told that I should use XRay instead of UT. Tubes are 20", 16", 12" 4" and 3", both with butt weld.
Regards
Souza
Does anyone tell me what kind of 316 L tubes weld inspection according to ASME? I was told that I should use XRay instead of UT. Tubes are 20", 16", 12" 4" and 3", both with butt weld.
Regards
Souza





RE: 316 L
What is the ASTM/ASME material specification for the tubing? This will answer your question.