Does anyone have friction coefficients for duplex 2205 on duplex 2205?
I suspect that I am going to have to run a few tests to determine it, but some preliminary guidance would be nice.
thanks
DRW
(not sure if this is the correct forum but...)
Does anyone have friction coefficients for duplex 2205 on duplex 2205?
I suspect that I am going to have to run a few tests to determine it, but some preliminary guidance would be nice.
thanks
DRW





RE: Duplex 2205 Friction
A Google search for 2205 duplex ss revealed 0.3-0.5 for the coefficient of friction under dry conditions. I would run your own tests to be sure.