INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Semi finished bolts

Semi finished bolts

Semi finished bolts

(OP)
Hi,
what are semi finished bolts?
I've done a google search with no luck.

Thank you

RE: Semi finished bolts

The unfinished thread is one example. Another is missing the hex head, I have seen recently a pack of Chinese bolts with Phillips head, missing the cross slots. No refund given...
cheers,
gr2vessels

RE: Semi finished bolts

(OP)
I have a drawing with this specification:

Stud Bolt, 1 1/8'' x 230mm, A193-B7 w/2
A194-2H Nuts, Semi-Finished.

Does this mean that the nuts are not done? Confusing.

Thank you.

RE: Semi finished bolts

Semi-finished nuts are tapped and one face finished flat, perpendicular to the thread.  From American Machinists' Handbook.

Ted

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources