INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

BHN requirements

BHN requirements

BHN requirements

(OP)
Is it a true statement that BHN testing is not required by B31.1?  

RE: BHN requirements

Yes. Hardness testing, if required, is usually indicated by material specification with an acceptable hardness range.

RE: BHN requirements

Please note that there is an exception to this case when dealing with P92 material (250 max BHN).  Code case 183.

RE: BHN requirements

B31.3 para 331.1.7 and Table 331.1.1. specify when hardness testing is required.  

Nigel Armstrong
Karachaganak Petroleum
Kazakhstan

RE: BHN requirements

While B31.1 does not require hardness testing, many owners and engineers do require it for welds in P91. As a Contractor, we have required hardness testing of our P91 welds for over ten years.  

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.