What is the correct way to call out nylon 6/6 with 33% glass fill?
What is the correct way to call out nylon 6/6 with 33% glass fill?
(OP)
The way we mark an ABS part is: <ABS>
1) What is the name of the standard in which materials are called out this way?
2) to callout nyclon 6/6 with 33% glass fill, is it <PA66GF33> ?
Thanks
1) What is the name of the standard in which materials are called out this way?
2) to callout nyclon 6/6 with 33% glass fill, is it <PA66GF33> ?
Thanks





RE: What is the correct way to call out nylon 6/6 with 33% glass fill?
The standards include:
ISO 1043-1—Plastics-Symbols—Part 1: Basic polymers and their special characteristics
ISO 1043-2—Plastics-Symbols—Part 2: Fillers and reinforcing materials
ISO 1629—Rubber and latices—Nomenclature
ISO 11469—Plastics—Generic identification and marking of plastic products
SAE J1344 MARKING OF PLASTIC PARTS
Regards,
Cory