INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

magnesium oxidizing

magnesium oxidizing

magnesium oxidizing

(OP)
hi everybody;

i try to oxidize magnesium in hot water but i have small time to do it so i want to add a salt in to water for rapidly oxidizing.

I search which salt must I add to rapidly oxidize magnesium.

If you have an idea i will be happy

thanks

RE: magnesium oxidizing

Why do you want to oxidize magnesium?  That will determine how we can provide tips to help you.

Regards,

Cory

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of Eng-Tips Fora.

RE: magnesium oxidizing

(OP)
        
          First I will oxidize mg than melt with flux5 and than I am going to try to recycle mg.

Sincerely

RE: magnesium oxidizing

You are talking about a large scale operation to recycle any quanity of magnesium scrap. I think it would be best to purhase a process.  

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources