INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

What code for stainless steel welding?

What code for stainless steel welding?

What code for stainless steel welding?

(OP)
hi Folks

Could anyone help me find a code that specifies welding procedures, welder qualification and defect acceptance criteria for 316 stainless steel.

kind regards

JWC
Mechanical/Structural
Brisbane, Australia

RE: What code for stainless steel welding?

Codes don't generally specify welding procedures.  But ASME Boiler and Pressure Vessel Code and API 650 are two standards that include stainless steel.

RE: What code for stainless steel welding?

For structural applications AWS D1.6 can be used for guidance, containing prequalified WPS', welder qualification, and acceptance/reject criteria.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources