Chrome Depletion 304H welds
Chrome Depletion 304H welds
(OP)
Hello all,
I have evidence of chromium depletion in 304H butt welds from metallurgical analysis. The depletion appears to be the result of high heat input / slow cooling.
I want to develop a presentation for our trades people and wondering if there are any "canned" materials out there similar to this.
I have evidence of chromium depletion in 304H butt welds from metallurgical analysis. The depletion appears to be the result of high heat input / slow cooling.
I want to develop a presentation for our trades people and wondering if there are any "canned" materials out there similar to this.





RE: Chrome Depletion 304H welds
http://serkanakinci.tripod.com/id17.html
http://www.weldreality.com/stainlesswelddata.htm
RE: Chrome Depletion 304H welds
http://as
S.
Corrosion Prevention & Corrosion Control
RE: Chrome Depletion 304H welds