info on 38Mnv56
info on 38Mnv56
(OP)
Hi
i have got some 38Mnv56 and would like to heat treat it to conform to ISO 898 gr 8.8 would it be possible to achieve this with this material and if so could you give me the heat treatment requirements
i have got some 38Mnv56 and would like to heat treat it to conform to ISO 898 gr 8.8 would it be possible to achieve this with this material and if so could you give me the heat treatment requirements





RE: info on 38Mnv56
http://www.metaldata.info/eng/sinquiry.php
If you have the MTR, I would query the manufacturer directly for product data sheet.
RE: info on 38Mnv56
RE: info on 38Mnv56