INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

thread class - 3A screw in 2B hole?

thread class - 3A screw in 2B hole?

thread class - 3A screw in 2B hole?

(OP)
hello,

i'm wondering if anybody can share some thoughts on mixing thread classes.  specifically, what would be the potential problems versus a 'proper' class 2 or class 3 thread.  thanks!

  

RE: thread class - 3A screw in 2B hole?

Class 3 in class 3 allows a line fit at max tolerance as I recall.

Class 2 in class 2 always has a certain amount of clearance.

A class 3 screw in a class 2 hole will have a fit somewhere between these 2.  So, simplistically, it will be 'tighter' than a 2 in a 2 but looser than a 3 in a 3.

It will be more tolerant of 'contamination' in between threads than a 3-3, but not as tolerant as a 2-2.

Take a look at ASME B1.1 to better understand unified thread tolerances.

What is your application?

KENAT, probably the least qualified checker you'll ever meet...

RE: thread class - 3A screw in 2B hole?

I have mix the thread class in the passed and have nor problems.  Take a look at the ASME.

Chris

"In this house, we obey the laws of thermodynamics." Homer Simpson

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources