INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Inconel 718 Hardness Data

Inconel 718 Hardness Data

Inconel 718 Hardness Data

(OP)
Folks....

I need Rockwell Hardness data for Inconel 718 in the following forms [or equivalent]:

Inconel 718 per AMS5662: Solution HT
Inconel 718 per AMS5663: Solution HT & Precipitation HT

NOTE: I need MIN and MAX hardness values for range comparison.

NOTE: If You know the MIN and MAX corresponding FTy [relative to hardness] I would also appreciate this info.

Regards, Wil Taylor

RE: Inconel 718 Hardness Data

Wil,

I was going to try to dig some stuff up for you, but apparently Special Metals has put a ton of info on their website.  For Inconel 718, the exact link is:

http://www.specialmetals.com/publication/tech_bulletin_718.pdf

I briefly scanned the 26 pages, and it looks like it has what you are looking for.

RE: Inconel 718 Hardness Data

(OP)
Hush & TVP...

The Special Metals website You both listed has the exact Info I was looking for... and much more!

Regards, Wil Taylor

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources