INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Where can I find thermal expansion data for ASTM A216 WCB / WCC?

Where can I find thermal expansion data for ASTM A216 WCB / WCC?

Where can I find thermal expansion data for ASTM A216 WCB / WCC?

(OP)
Hi guys and gals,



Trying to find the coefficient of thermal expansion for ASTM A216 WCB and WCC and my usual source (MATWEB) for this data has let me down!

Can any of you good people point me in the right direction please?


Thanks in advance,


Jon

RE: Where can I find thermal expansion data for ASTM A216 WCB / WCC?

You can still use Matweb. This is a cast carbon steel, probably similar to a 1030 wrought carbon steel for an approximation. Go to Matweb and find the linear CTE.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources