Temperature Degraded properties for AISI 4140
Temperature Degraded properties for AISI 4140
(OP)
Hi,
I am trying to find temperature dependent properties for AISI 4140 Steel. Mainly looking for its Yield Strength at 400 F temperature. Does anyone know of any resources I can use?
Thanks,
Mike
I am trying to find temperature dependent properties for AISI 4140 Steel. Mainly looking for its Yield Strength at 400 F temperature. Does anyone know of any resources I can use?
Thanks,
Mike





RE: Temperature Degraded properties for AISI 4140
RE: Temperature Degraded properties for AISI 4140
My guess was that it should be within 8 to 10% too, but isn't there any resource that cites such data. I mean a plot of temperature vs yield?
RE: Temperature Degraded properties for AISI 4140
RE: Temperature Degraded properties for AISI 4140
Thanks!
Mike
RE: Temperature Degraded properties for AISI 4140
http: