I have a condition where a 1/4" fillet weld has already been made. Now, a 5/16" fillet weld is required. Is it acceptable to just ad the additional 1/16" of weld?
Thanks!
Thanks!





RE: adding to existing fillet weld
You don't say how thick your metal components are, but your fillet weld size cannot exceed the thickness of the smallest section within the joint.
Regards
desertfox
RE: adding to existing fillet weld
RE: adding to existing fillet weld
Yes, provided you add filler metal to make the existing fillet legs equal in size for a 5/16" weld.
RE: adding to existing fillet weld
RE: adding to existing fillet weld
Hg