INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

What's the purpose of hydrogen probe installed.....

What's the purpose of hydrogen probe installed.....

What's the purpose of hydrogen probe installed.....

(OP)
I'm currently working in refinery industry.
I have had something to see what is the purpose of hydrogen probe installed on pressure vessure.

The name of pressure vessels are primary and sponge absorber,lean gas knock out drum,stripper,debuthanizer.

 

RE: What's the purpose of hydrogen probe installed.....

hydrogen is throughout the refinery and it ends up in the light ends.  Hydrogen is not friendly to vessels and they must be checked periodically to see if hydrogen is present and is actively impinging the vessels which may lead to vessels failing.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources